CH EN

Al₂O₃(%)-SiC-C Iron runner

Class performanceT-1T-2
Al2O3(%)65-7040-60
SiC(%)10-2010-20
SiO2(%)2-510-25
F.C(%)3-85-12
Bulk density(g/cm³)110℃x24h2.95-3.12.85-2.95
1450℃x3h

2.85-2.9

2.7-2.8
Compressive strength(Mpa)110℃x24h≥40≥30
1450℃x3h≥55≥45
Flexural strength(Mpa)110℃x24h≥5≥4
1450℃x3h≥8≥6
Linear change rate(%)1500℃x3h±0.5±1.0
Use parts and construction methodsFor large blast furnace main ditch, slag ditch and other on-site ramming or pouringFor small and medium blast furnace main ditch, slag ditch and other on-site ramming or pouring